Stainless steel 321H seamless tubes and pipes are titanium stabilized austenitic steel products for high-temperature service. The SS 321H seamless tube has a chemical composition of 17 to 19% chromium and 9 to 12% nickel, with titanium added and the carbon controlled between 0.04 and 0.10%. The titanium stops the 321H seamless pipe from sensitizing when it is held between 800 and 1500°F (425 and 815°C). The higher carbon gives the TP321H tube better creep strength than standard 321. The 321H stainless steel tube has a minimum tensile strength of 75 ksi and a minimum yield strength of 30 ksi. SS 321H seamless tubes and pipes are used in superheaters, reheaters, refinery heaters, hydrotreaters, expansion joints, exhaust systems, etc. USA Piping Solution is a supplier of stainless steel 321H seamless tube and pipe in the USA. We supply these products with mill test certificates.
Why 321H Is Used at 800 to 1500°F
Unstabilized grades such as 304H form chromium carbides in this temperature range. After shutdown, the sensitized steel can crack in the presence of moisture and sulfur compounds. Refineries call this polythionic acid stress corrosion cracking. In 321H the titanium forms carbides in place of the chromium, so the tube keeps its corrosion resistance. This is the reason 321H is used for refinery heater tubes and transfer lines.
321 vs 321H
|
Point |
321 |
321H |
|---|---|---|
|
UNS |
S32100 |
S32109 |
|
Carbon |
0.08% max |
0.04 to 0.10% |
|
Titanium (min) |
5 x (C + N) |
4 x (C + N) |
|
Grain size |
No requirement |
ASTM No. 7 or coarser |
|
Best use |
Welded parts up to about 1000°F |
Pressure parts above about 1000°F |
The standard grade is on the SS 321 Seamless Tubes page.
Applications
- Power boilers: superheater and reheater tubes. Other grades are on the Boiler Tubes & Pipes page.
- Refineries: heater tubes, transfer lines and hydrotreater piping.
- Chemical plants: hot process lines and heat exchangers.
- Exhaust and expansion joints: parts that cycle through the sensitizing range.
Testing & Documentation
SS 321H seamless tubes and pipes are supplied with a mill test certificate. The certificate shows the heat number, chemical analysis with the titanium content, tensile results and grain size. Each length is hydrostatically tested or tested by a non-destructive electric test. Our Quality Policy page explains how incoming material is checked.
Related Products
SS 321 Seamless Tubes · 347H Stainless Steel Seamless Pipe & Tube · SS 304H Seamless Pipe & Tube
Frequently Asked Questions
1. What is the difference between 321 and 321H stainless steel?
321H has a controlled carbon content of 0.04 to 0.10% and a grain size requirement. This gives it better creep strength at high temperature.
2. Why is titanium added to 321H?
Titanium combines with carbon and stops chromium carbides from forming. The steel then keeps its corrosion resistance after long heating.
3. What temperature is 321H used at?
321H is used for parts that work between about 800 and 1500°F (425 and 815°C). The limit for a pressure part comes from the design code.
4. Is 321H the same as 347H?
No. 321H is stabilized with titanium and 347H is stabilized with niobium. Both resist sensitization.